| Metric | S30V | D2 |
|---|---|---|
| Toughness | 4 | 3.5 |
| Edge Retention | 6 | 5 |
| Corrosion Resistance | 7.5 | 4.5 |
| Avg/Target HRC | 59.6 | 59.7 |
| Manufacturer | Crucible Industries | Various |
| Category | Stainless | High Alloy Tool Steel |
S30V vs D2
S30V vs D2 knife steel comparison using sourced ratings and hardness data from Knife Steel Nerds and SteelHardnessLab.
Quick Take
- Toughness: S30V leads (4/10 vs 3.5/10 for D2).
- Edge retention: S30V leads (6/10 vs 5/10 for D2).
- Corrosion resistance: S30V leads (7.5/10 vs 4.5/10 for D2).
Also searched as: S30V (CPM-S30V)
Also searched as: D2 (Bohler K110, CPM-D2)
FAQ
Is S30V better than D2 overall?
Toughness: S30V leads (4/10 vs 3.5/10 for D2). Edge retention: S30V leads (6/10 vs 5/10 for D2). Corrosion resistance: S30V leads (7.5/10 vs 4.5/10 for D2).
Where do these values come from?
Ratings are attributed to Knife Steel Nerds; hardness measurements are attributed to SteelHardnessLab testing by u/679696 and u/Skylark427.