| Metric | Nitro-V | 3V |
|---|---|---|
| Toughness | 7.5 | 9 |
| Edge Retention | 3 | 4.5 |
| Corrosion Resistance | 8.5 | 5.5 |
| Avg/Target HRC | 58.8 | 60.7 |
| Manufacturer | Bohler-Uddeholm | Crucible Industries |
| Category | Stainless | High Alloy Tool Steel |
Nitro-V vs 3V
Nitro-V vs 3V knife steel comparison using sourced ratings and hardness data from Knife Steel Nerds and SteelHardnessLab.
Quick Take
- Toughness: 3V leads (9/10 vs 7.5/10 for Nitro-V).
- Edge retention: 3V leads (4.5/10 vs 3/10 for Nitro-V).
- Corrosion resistance: Nitro-V leads (8.5/10 vs 5.5/10 for 3V).
Also searched as: Nitro-V (Nitro V, Bohler Nitro-V)
Also searched as: 3V (CPM 3V, CPM-3V)
FAQ
Is Nitro-V better than 3V overall?
Toughness: 3V leads (9/10 vs 7.5/10 for Nitro-V). Edge retention: 3V leads (4.5/10 vs 3/10 for Nitro-V). Corrosion resistance: Nitro-V leads (8.5/10 vs 5.5/10 for 3V).
Where do these values come from?
Ratings are attributed to Knife Steel Nerds; hardness measurements are attributed to SteelHardnessLab testing by u/679696 and u/Skylark427.