METALLURGY.INFO
arrow_back All Steels

Stainless / Bohler-Uddeholm

N690

Toughness 3.5/10, Edge Retention 4.5/10, Corrosion Resistance 8/10. Target hardness range: 58-61 HRC.

Known aliases: Bohler N690.

Technical Summary

  • CategoryStainless
  • ManufacturerBohler-Uddeholm
  • ProcessIngot
  • HRC Range58-61

Ratings: Toughness 3.5, Edge 4.5, Corrosion 8

Source attribution: Knife Steel Nerds and SteelHardnessLab.

Chemical Composition

C1.07%
Cr17.3%
V0.1%
Mo1.1%
Co1.5%

SteelHardnessLab Testing Data

Testing recognition: u/679696 and u/Skylark427.

ManufacturerSamplesAvg HRC
GiantMouse160.0
TOPS159.4
Kizer357.8

Heat Treat Data

Austenitize 1940F, quench PLATE, temper 175F.